Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 200 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 300 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge An opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings. 331W has same properties as 331 with the only ex.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 475 Polyester Film, 200 Gauge Melinex® 475 is a high yield, translucent polyester film with superb handling properties. Both surfaces are pretreated to promote adhesion to most industrial coatings.General Product Info: This fil.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Mylar® C Polyester Film, 14 Gauge Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 500 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge Melinex® 487 is a high-yield, white film that is coated on one side for adhesion to inks, coatings, laser printing, and thermal transfer printing.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MLB Polyester Film, 300 Gauge Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML.. |