Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 13.5 MPa | 1960 psi | Calculated from mfr's report of 35 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Film Tensile Strength at Break, MD | 13.5 MPa | 1960 psi | ASTM D3759 |
3M Scotch® 640 Transparent Film Tape Scotch® 640 is a transparent film tape used for sealing, tabbing, splicing, various inner-pack applications and garment applications. This product has a conformable backing and a consistent pressur.. |