Polymer Property : Film Tensile Strength at Break, MD = 13.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 13.5 MPa
1960 psi
Calculated from mfr's report of 35 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Film Tensile Strength at Break, MD 13.5 MPa
1960 psi
ASTM D3759
3M Scotch® 640 Transparent Film Tape
Scotch® 640 is a transparent film tape used for sealing, tabbing, splicing, various inner-pack applications and garment applications. This product has a conformable backing and a consistent pressur..