Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M Scotch® 3743 High Tack Box Sealing Tape
Scotch® Box Sealing Tape 3743 is a high-tack packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a heavy-duty, conformable backin..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M Scotch® 824 Pouch Tape
Scotch® Pouch Tape 824 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M Scotch® 825 Pouch Tape
Scotch® Pouch Tape 825 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M ScotchPad™ 830 Pouch Tape Pads
3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M ScotchPad™ 832 Pouch Tape Pads
3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M ScotchPad™ 832CP Pouch Tape Pads
3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M Scotch® 827 Pouch Tape
Scotch® Pouch Tape 827 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible..
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
3M ScotchPad™ 830CP Pouch Tape Pads
3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl..