Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M Scotch® 3743 High Tack Box Sealing Tape Scotch® Box Sealing Tape 3743 is a high-tack packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a heavy-duty, conformable backin.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M Scotch® 824 Pouch Tape Scotch® Pouch Tape 824 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M Scotch® 825 Pouch Tape Scotch® Pouch Tape 825 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M ScotchPad™ 830 Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M ScotchPad™ 832 Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M ScotchPad™ 832CP Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M Scotch® 827 Pouch Tape Scotch® Pouch Tape 827 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Film Tensile Strength at Break, MD | 7.95 MPa | 1150 psi | ASTM D3759 |
3M ScotchPad™ 830CP Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |