Polymer Property : Elmendorf Tear Strength MD = 95 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 95 g
95 g
ASTM D1922
Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin  (discontinued **)
Low Density, Linear Polyethylene Film ResinCustomer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of to..
Elmendorf Tear Strength MD 95 g
95 g
ASTM D1922
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..