Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density, Linear Polyethylene Film ResinCustomer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of toughness and tensile. D252/257 may be used straight, in blends, or coextruded with HMW-HDPE, LLDPE, and LDPE. It is especially well suited in blends with LLDPE to increase melt strength and processing rate of LLDPE. In thick gauge heavy duty applications, the benefit of the high molecular weight tail is seen in puncture resistance. Processing is excellent on many types of equipment and under a variety of conditions, including high stalk. Meets FDA regulations for food packaging below cooking temperatures. D256 contains premium stabilizer.Applications: Heavy wall bagsProperty Comments: HDPE line, 4:1 BUR, .035" gap, 8" die, 56" FLH, 240 lbs/hr, 420°FData provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 0.30 g/10 min
0.30 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 15.0 MPa
2180 psi
2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa
1890 psi
2 in per min; ASTM D882
Film Elongation at Break, MD 500 %
500 %
2 in per min; ASTM D882
Film Elongation at Break, TD 600 %
600 %
2 in per min; ASTM D882
Elmendorf Tear Strength MD 95 g
95 g
ASTM D1922
Elmendorf Tear Strength TD 450 g
450 g
ASTM D1922
Dart Drop Test 350 g
0.772 lb
26 in; ASTM D1709
Film Tensile Strength at Break, MD 45.0 MPa
6530 psi
2 in per min; ASTM D882
Film Tensile Strength at Break, TD 43.0 MPa
6240 psi
2 in per min; ASTM D882