Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 825 g
825 g
ASTM D1922
Dow ELITE™ 5400G Enhanced Polyethylene Resin
™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc..
Elmendorf Tear Strength MD 825 g
825 g
ASTM D1922
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..