Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 60 g | 60 g | Orientation not specified; ASTM D1922 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | Orientation not specified; ASTM D1922 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D1922 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D1922 |
Iran Petrochemical (PCC) 16503 Linear Low Density Polyethylene 16503 is a LLDPE for general purpose cast stretch film grade. The ease of processing and the low gels make 16503 well suited for production of general purpose monolayer or multilayer cast stretch fi.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D1922 |
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D1922 |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM-D1922 |
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer LF320 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It was developed for cast film extrusion. Films obtained with this product show a good processin.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM-D1922 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
Elmendorf Tear Strength MD | 60 g | 60 g | ASTM D1922 |
ExxonMobil Escorene® LD-713 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App.. |