Polymer Property : Elmendorf Tear Strength MD = 5.0 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 5.0 g
5.0 g
Orientation not specified; ASTM D1922
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Elmendorf Tear Strength MD 5.0 g
5.0 g
ASTM-D1922
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer
HD3000N is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for cast film extrusion. It offers high processability, stiffness, and good impact resist..