Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin) , Polypropylene (PP)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when excellent optics, high shrink force, and superb sheet flatness are essential. An excellent choice for doing multi-packs, high-speed applications, and static sealing.
Physical Properties Metric English Comments
Oxygen Transmission 92.0 cc-mm/m²-24hr-atm
234 cc-mil/100 in²-24hr-atm
or 6100 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 130 %
130 %
Average; ASTM D882
Modulus of Elasticity 0.770 GPa
112 ksi
(stiffness), ASTM D882
Coefficient of Friction, Dynamic 0.45
0.45
ASTM D1894
Elmendorf Tear Strength MD 5.0 g
5.0 g
Orientation not specified; ASTM D1922
Seal Strength 2500 g/25 mm
2500 g/in
F-88-68(73)
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
Gloss 150 %
150 %
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Optimum Tunnel temperature range.