Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 43 g | 43 g | ASTM D1922 |
Huntsman Rexell® M3105 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of toughness, stiffness, and water vapor barrier with good temperature resistance.Applications:.. |