Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 42 g | 42 g | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |