Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow AFFINITY™ HF 1030 Polyolefin Plastomer

Category Polymer , Film , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name AFFINITY™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow AFFINITY™ HF 1030 Polyolefin Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds, and exceptional resistance to draw resonance. It can bring important value to a variety of personal care and medical applications as high performance monolayer films or coextruded films. AFFINITY HF 1030 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. AFFINITY HF 1030 polymer complies with FDA regulation 21 CFR 177.1520c3.2a, which allows for its use in direct food contact applications.Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Thickness 25.0 microns
0.984 mil
Melt Flow 2.5 g/10 min

@Load 2.16 kg
2.5 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 9.5.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.4 MPa
1650 psi
Film Tensile Strength at Yield, TD 10.9 MPa
1580 psi
Film Elongation at Break, MD 530 %
530 %
Film Elongation at Break, TD 580 %
580 %
Secant Modulus, MD 0.200 GPa
29.0 ksi
Film value
Secant Modulus, TD 0.214 GPa
31.0 ksi
Film value
Elmendorf Tear Strength MD 42 g
42 g
Elmendorf Tear Strength TD 118 g
118 g
Elmendorf Tear Strength, MD 1.70 g/micron
43.2 g/mil
Elmendorf Tear Strength, TD 4.70 g/micron
119 g/mil
Film Tensile Strength at Break, MD 29.6 MPa
4290 psi
Film Tensile Strength at Break, TD 22.8 MPa
3310 psi
Processing Properties Metric English Comments
Processing Temperature 274 °C
525 °F
Film extrusion temperature
Copyright © lookpolymers.com All Rights Reserved