Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 385 g | 385 g | |
Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA reg.. |
|||
Elmendorf Tear Strength MD | 385 g | 385 g | |
Dow ATTANE™ 4601 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4601 copolymer is an ultra low density polyethylene blown film extrusion grade having high impact resistance and tear strength combined with improved softness, designed for use in medical p.. |