Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Dow Chemical
Trade Name ATTANE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow ATTANE™ 4201 Ultra Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ATTANE® 4201 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a, allowing for use in packing or holding food during cooking when used unmodified and according to good manufacturing practices for food contact application.Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.912 g/cc
0.0329 lb/in³
Moisture Vapor Transmission 0.0300 cc-mm/m²-24hr-atm
0.0762 cc-mil/100 in²-24hr-atm
or 1.2 g/m²/atm/24 hr
Thickness 25.0 microns
0.984 mil
Melt Flow 1.0 g/10 min

@Load 2.16 kg
1.0 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.2.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 385 g
385 g
Elmendorf Tear Strength TD 499 g
499 g
Elmendorf Tear Strength, MD 15.4 g/micron
391 g/mil
Elmendorf Tear Strength, TD 20.0 g/micron
508 g/mil
Dart Drop >= 33.2 g/micron
>= 843 g/mil
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
Processing Properties Metric English Comments
Processing Temperature 96.0 °C
205 °F
Seal initiation temperature
226 °C
439 °F
Film extrusion temperature