Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene 12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |
|||
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |