Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 107 g | 107 g | ASTM D1922 |
LyondellBasell Petrothene® NA350136 Low Density Polyethylene ApplicationsPETROTHENE NA 350-136 is a low density/EVA copolymer designed for heavy duty film packaging and other high strength, easy to seal packaging. NA 350-136 exhibits high impact strength and.. |