Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA350136 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA350136 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 350-136 is a low density/EVA copolymer designed for heavy duty film packaging and other high strength, easy to seal packaging. NA 350-136 exhibits high impact strength and good low temperature toughness. It contains Medium levels of Slip and High levels of Antiblock.Regulatory StatusThe base resin NA 350-136 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1350. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions use may apply.ProcessingSpecific recommendations for processing NA 350-136 can only be made when the processing conditions, equipment and end use are known.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D1505
Vinyl Acetate Content 6.6 %
6.6 %
Thickness 31.8 microns
1.25 mil
2:1 BUR
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
ASTM D882
Film Elongation at Break, TD 470 %
470 %
ASTM D882
Elmendorf Tear Strength MD 107 g
107 g
ASTM D1922
Elmendorf Tear Strength TD 83 g
83 g
ASTM D1922
Dart Drop Test 285 g
0.628 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 22.4 MPa
3250 psi
ASTM D882
Film Tensile Strength at Break, TD 19.0 MPa
2750 psi
ASTM D882
1% Secant Modulus, MD 138 MPa
20000 psi
ASTM D882
1% Secant Modulus, TD 159 MPa
23000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003
Gloss 55 %
55 %
45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 221 °C
430 °F