Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 1.4 g
1.4 g
ASTM D1922
Chevron Phillips MarFlex® 9608 HDPE Coating Blend Resin
Resin Type: Coating Blend ResinCharacteristics: Low Gel Levels, Improves MVTR, Reduces COF, Excellent Draw Properties, Excellent Processability, Improves Scuff Resistance, Improves Stiffness Propert..