Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.02797 GPa
4.056 ksi
ASTM D412 Method A
Seals Eastern 7204 Ethylene-Propylene Rubber
Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc.