Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.02797 GPa | 4.056 ksi | ASTM D412 Method A |
Seals Eastern 7204 Ethylene-Propylene Rubber Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc. |