Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.230 - 0.689 GPa | 33.4 - 100 ksi | Average value: 0.431 GPa Grade Count:10 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Secant Modulus | 0.230 - 0.448 GPa | 33.4 - 65.0 ksi | Average value: 0.354 GPa Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |