Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0210 - 1.25 GPa | 3.05 - 181 ksi | Average value: 0.496 GPa Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Secant Modulus | 0.786 - 1.25 GPa | 114 - 181 ksi | Average value: 0.999 GPa Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |