Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.00539 GPa | 0.782 ksi | ASTM D412 Method A |
Seals Eastern 5242 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Secant Modulus | 0.00539 GPa | 0.782 ksi | ASTM D412 Method A |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |