Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 9.03 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |
|||
Film Tensile Strength at Yield, MD | 9.03 MPa | 1310 psi | ASTM D882 |
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin
(discontinued **) Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals |