Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 1002.32 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 1002x74 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 1002x79 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | at 2% offset; ASTM D882 |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | ASTM D882 |
ExxonMobil LL 1002.09 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Film Tensile Strength at Yield, MD | 8.48 MPa | 1230 psi | at 2% offset; ASTM D882 |
ExxonMobil LL 1002x75 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |