Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 7.24 MPa | 1050 psi | ASTM D882 |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |