Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 7.10 MPa
1030 psi
ASTM D882
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and..
Film Tensile Strength at Yield, MD 7.10 MPa
1030 psi
at 2% offset; ASTM D882
ExxonMobil Escorene® LD 712.06 Film Resin  (discontinued **)
Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular..