Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 68.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 68.0 MPa
9860 psi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU)
Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU ..
Film Tensile Strength at Yield, MD 68.0 MPa
9860 psi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- Udel® PSU P-1700 NT-11 Polysulfone (PSU)
Udel® P-1700 polysulfones are tough, high-strength thermoplastics that are suitable for continuous use up to 300°F (149°C). Udel Film is resistant to oxidation and hydrolysis and withstand ..
Copyright © lookpolymers.com All Rights Reserved