Polymer Property : Film Tensile Strength at Yield, MD = 6.89 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
at 2% offset; ASTM D882
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
at 2% offset; ASTM D882
ExxonMobil Escorene® LD 319.92 Film Resin  (discontinued **)
Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil LL 3003.32 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil LL 3003.39 Cast Film Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil LLDPE LL 3003.32 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin
Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p..
Film Tensile Strength at Yield, MD 6.89 MPa
1000 psi
ASTM D882
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..
Film Tensile Strength at Yield, MD 6.89 - 28.0 MPa
1000 - 4060 psi
Average value: 11.1 MPa Grade Count:131
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..