Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | >= 45.0 MPa | >= 6530 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, MD | >= 45.0 MPa | >= 6530 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, MD | 45.0 MPa | 6530 psi | ASTM D882 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Film Tensile Strength at Yield, MD | >= 45.0 MPa | >= 6530 psi | ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Film Tensile Strength at Yield, MD | 45.0 MPa | 6530 psi | ASTM D882 |
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used.. |