Polymer Property : Film Tensile Strength at Yield, MD = 3990 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 27.5 MPa
3990 psi
ISO 527-3
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra..
Film Tensile Strength at Yield, MD 27.5 MPa
3990 psi
Dow HDPE 05862N High Density Polyethylene
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.