Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 17.2 MPa | 2500 psi | ASTM D882 |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |