Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 25.5 MPa | 3700 psi | ASTM D882 |
LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade ALATHON H6012 is medium molecular weight high density polyethylene homopolymer for use in cast film applications. Typical applications for this resin include extrusion coating, blends with LDPE and .. |
|||
Film Tensile Strength at Yield, MD | 25.5 MPa | 3700 psi | ASTM D882 |
LyondellBasell Alathon® L5485 High Density Polyethylene ApplicationsALATHON L 5485 is a medium molecular weight, high density polyethylene copolymer for use in blown film applications. Typical applications include general purpose HDPE film applications .. |
|||
Film Tensile Strength at Yield, MD | 25.5 MPa | 3700 psi | ASTM D882 |
LyondellBasell Alathon® L5885 High Density Polyethylene ApplicationsALATHON L 5885 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include those low WVTR requirements.Regulatory StatusL 5855.. |