Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® H6012 High Density Polyethylene, MMW Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ALATHON H6012 is medium molecular weight high density polyethylene homopolymer for use in cast film applications. Typical applications for this resin include extrusion coating, blends with LDPE and laminations. Regulatory Status: H6012 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for further information regarding the suitability of specific products for specific applications.Specific recommendations for processing H6012 can only be made when the processing conditions, equipment and end use are known. For further suggestions please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 25.5 MPa
3700 psi
ASTM D882
Film Tensile Strength at Yield, TD 31.7 MPa
4600 psi
ASTM D882
Film Elongation at Break, MD 850 %
850 %
ASTM D882
Film Elongation at Break, TD 350 %
350 %
ASTM D882
Secant Modulus, MD 0.932 GPa
135 ksi
ASTM D882
Secant Modulus, TD 1.07 GPa
155 ksi
ASTM D882
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
Chill Roll
Melt Temperature 177 °C
350 °F