Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Informati.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Film Tensile Strength at Yield, MD | 103 MPa | 15000 psi | ASTM D882A |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 103 MPa @Strain 5.00 % |
15000 psi @Strain 5.00 % |
ASTM D882 |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |