DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 103 MPa
15000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 103 MPa
15000 psi
ASTM D882A
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
A-B; ASTM D1894
Film Tensile Strength at Break, MD 228 MPa
33000 psi
ASTM D882A
Film Tensile Strength at Break, TD 248 MPa
36000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.5 %

@Temperature 190 °C,
Time 300 sec
3.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.3 %

@Temperature 190 °C,
Time 300 sec
2.3 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 87 %
87 %
TLT; ASTM D1003