Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 89.6 MPa
13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 054 Polyester Film
Melinex® 054 is a high clarity, low balanced shrink polyester film which is two-side pretreated to promote adhesion to industrial coatings and inks.Information provided by DuPont.
Film Tensile Strength at Yield, MD >= 89.6 MPa
>= 13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 461 Polyester Film
Melinex® 461 is a high clarity polyester film manufactured with a coating on one surface that promotes adhesion to many solvent formulations and to most vinyl or acrylic base ink systems. The adhes..
Film Tensile Strength at Yield, MD >= 89.6 MPa
>= 13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 473 Polyester Film, 200 Gauge
Melinex® 473 is a high clarity polyester film manufactured with a coating on one surface that improves slip and handling characteristics. The opposite surface is raw polyester (non-coated). The sli..
Film Tensile Strength at Yield, MD >= 89.6 MPa
>= 13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 478 Polyester Film, 200 Gauge
Melinex® 478 is a high clarity polyester film manufactured with a coating on both surfaces that improves slip and handling characteristicsTypical Applications: Melinex 478 is used in many general i..
Film Tensile Strength at Yield, MD 89.6 MPa
13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 725 Polyester Film
Melinex® 725 is a high clarity polyester film pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 725 exhibits improved performance in multi-pass printing a..
Film Tensile Strength at Yield, MD 89.6 MPa
13000 psi
ASTM D882A
DuPont Teijin Films Melinex® 523 Polyester Film
Melinex® 523 is a high clarity polyester film. It is pretreated on both surfaces with MAP (multiple application pretreatment) to promote adhesion to most aqueous and solvent coating formulations. I..