Polymer Property : Film Tensile Strength at Yield, MD = 1240 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.55 MPa
1240 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin
Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness..