ExxonMobil Exceed™ 2718CB Premium Cast Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Exceed™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exceed™ 2718CB Premium Cast Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness. These superior properties, along with excellent drawability, make this a versatile resin for both monolayer and multilayer cast stretch film.Availability: Europe, Latin America, North America and South AmericaAdditive: Antiblock: NoSlip: NoProcessing Aid: NoThermal Stabilizer: YesApplications: Bag in BoxBarrier Food PackagingBlown FilmCast FilmCast Stretch FilmDiaper BacksheetForm Fill and Seal PackagingHygiene FilmPackaging FimsPersonal CarePremium Trash BagsStand Up PouchesInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 20.3 microns
0.800 mil
Melt Flow 2.7 g/10 min
2.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.55 MPa
1240 psi
at 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 7.86 MPa
1140 psi
at 2% offset; ASTM D882
Film Elongation at Break, MD 470 %
470 %
ASTM D882
Film Elongation at Break, TD 720 %
720 %
ASTM D882
Puncture Energy 4.18 J
3.08 ft-lb
Exxon Mobil Method
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
Elmendorf Tear Strength TD 420 g
420 g
ASTM D1922
Elmendorf Tear Strength, MD 8.366 g/micron
212.5 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 20.7 g/micron
525 g/mil
ASTM D1922
Dart Drop 8.366 g/micron
212.5 g/mil
ASTM D1709
Dart Drop Test 170 g
0.375 lb
ASTM D1709
Film Tensile Strength at Break, MD 75.08 MPa
10890 psi
ASTM D882
Film Tensile Strength at Break, TD 51.4 MPa
7450 psi
ASTM D882
1% Secant Modulus, MD 109 MPa
15800 psi
ASTM D882
1% Secant Modulus, TD 132 MPa
19100 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 117 °C
243 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
ASTM D1003
Gloss 91 %
91 %
45°; ASTM D2457
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: