Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.38 - 11.0 MPa
1360 - 1600 psi
Average value: 10.3 MPa Grade Count:3
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..