Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 101 MPa | 14600 psi | ASTM D882A |
DuPont Teijin Films Melinex® 514P Polyester Film This high clarity film has one side hydrophilic pretreated to promote adhesion to many solvent coatings formulations, while the opposite side is pretreated to provide antistatic protection.Informati.. |