Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.13333 MPa-m/sec
3806.6 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced
Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed..
Limiting Pressure Velocity 0.13333 MPa-m/sec
3806.6 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Copyright © lookpolymers.com All Rights Reserved