Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.13333 MPa-m/sec | 3806.6 psi-ft/min | v = 200m/min |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Limiting Pressure Velocity | 0.13333 MPa-m/sec | 3806.6 psi-ft/min | v = 200m/min |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |