Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | QTM 55007 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor |
Technetics Group Amicon™ Nylon 6/66
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor |
Technetics Group Amicon™ Acetal Homopolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |