Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
QTM 55007
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor
Technetics Group Amicon™ Nylon 6/66  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor
Technetics Group Amicon™ Acetal Copolymer  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Limiting Pressure Velocity 0.0946 MPa-m/sec
2700 psi-ft/min
4:1 safety factor
Technetics Group Amicon™ Acetal Homopolymer  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Copyright © lookpolymers.com All Rights Reserved