Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
4:1 safety factor
Technetics Group Amicon™ PEEK 30% Carbon  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
Unlubricated
TriStar CJ Composite Bearing
This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are..
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
Unlubricated
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
Unlubricated
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..
Limiting Pressure Velocity 0.875 MPa-m/sec
25000 psi-ft/min
at 0.35 m/s
A. Schulman ComAlloy E-16026N Internally Lubricated, Carbon Fiber Reinforced Polyester Alloy
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Limiting Pressure Velocity 0.876 MPa-m/sec
25000 psi-ft/min
Saint-Gobain Rulon® ACM Bearing/Seal PTFE  (discontinued **)
Saint Gobain Rulon® ACM is now produced as a part of the TriStar Plastics Corp. product line under the Ultracomp trade name.Description: This family of materials offers the combination of high comp..