Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Limiting Pressure Velocity = 22000 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.771 - 3.30 MPa-m/sec
22000 - 94200 psi-ft/min
Average value: 1.45 MPa-m/sec Grade Count:5
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Limiting Pressure Velocity 0.771 MPa-m/sec
22000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: ..
Limiting Pressure Velocity 0.771 MPa-m/sec
22000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro..
Limiting Pressure Velocity 0.771 MPa-m/sec
22000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf..
Limiting Pressure Velocity 0.771 MPa-m/sec
22000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance..
Limiting Pressure Velocity 0.771 MPa-m/sec
22000 psi-ft/min
1000 fpm
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta..
Limiting Pressure Velocity 0.770 MPa-m/sec
22000 psi-ft/min
at 0.35 m/s
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..