Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.666 MPa-m/sec | 19000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Limiting Pressure Velocity | 0.666 MPa-m/sec | 19000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Limiting Pressure Velocity | 0.666 MPa-m/sec | 19000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Limiting Pressure Velocity | 0.666 MPa-m/sec | 19000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |